Products > Copper Alloys > C67300 Products > C67300 Properties
H02 - Rod / Bar  - 
Tensile Strength:
Yield  Strength:
Elongation:
Rockwell Hardness B Scales:
75 ksi     
36 ksi - 0.5% Ext. under load         
26%            
78 
Chemical Composition  (%max., unless shown as range or min.)   
Need to send a drawing?
We are now accepting the following file types:
            Cu(1)        Al     Fe     Pb          Mn     Ni(2)     Si        Sn    Zn 
Min./Max.  58.0-63.0  .25   .50  .40-3.0  2.0-3.5   .25   .50-1.5   .30   Rem
Nominal    60.5              -       -     1.7        2.7             -     1.0            -     34.1  

(1) Cu value includes Ag.
(2) Ni value includes Co.
Note: Cu + Sum of Named Elements, 99.5% min. 
Joining Techniques
Soldering
Brazing
Oxyacetylene Welding
Gas Shielded Arc Welded
Coated Metal Arc Welding
Spot Weld
Seam Weld
Butt Weld
Capacity for Being Cold Worked
Machinability Rating
Suitability
Good
Not Recommended
Not Recommended
Fair
Not Recommended
Good
Good
Good
Fair
70
Mechanical Properties (measured at room temperature, 68 F (20 C) 
Fabrication Properties  
Typical for 2" Bar As Extruded Temper

Thermal Conductivity 
Specific Heat 
Thermal Expansion 
Density 
Electrical Conductivity* 
Modulus of Elasticity 
US Customary
58 BTU/ (sq ft-ft-hr-F) 58 
09 BTU/lb/ºF @ 68F . 
.000011  Per °F from 68 F to 572 F 
293  lb/cu in @ 68 F .
23 (Annealed) % IACS @ 68 F 
16,000  KSI 

Physical Properties