Products > Copper Alloys > C95520 Products > C95520 Properties
TH04 - As Continous Cast 
Tensile Strength:
Yield  Strength:
Elongation:
Brinell Hardness:

TQ30 - As Sand Cast
Tensile Strength:
Yield Strength:
Elongation:
Brinell Hardness:
Minimum 125 ksi     
-      
Minimum 2% in 2 in.           
262   3000 kg load


Minimum 125 ksi
Minimum 95 ksi - 0.5% Ext. under load
2%, in 2 inches
255   3000 kg load
Chemical Composition  (%max., unless shown as range or min.)   
Need to send a drawing?
We are now accepting the following file types:
  Cu                Al          Cr     Co       Fe       Pb   Mn    Ni(1)     Si     Sn     Zn  
Min./Max. 74.5 min  10.5-11.5   .05   .20   4.0-5.5   .03  1.5   4.2-6.0  .15    .25   .30
Nominal          -          11.0              -        -     4.7            -       -     5.1           -        -        -      

(1) Ni value includes Co.
Note: Cu + Sum of Named Elements, 99.5% min. 
Mechanical Properties (measured at room temperature, 68 F (20 C)